« Retour

Triplate

All standard plates are forged with a minimum compressive rate of 4.The plate design eliminates all welding.

All standard plate can be supplied with extra option:

  • zinc or aluminum anodes
  • «ORKOT LUYTEX» Insulating bushing and washers or equivalent.
  • Protection against corrosion: By zinc input >100 microns approx.or Epoxy Paint.
  • extra shackle for lifting / handling purposes in accordance with mooring line weight for installation .

 

Mechanical properties of steel

 

LE BEON No.pour  chaîne HRALHECMU TonCR/BL TonPoids Kg
CS SF = 4CS SF = 5
306 D 54 44 54 135 255 45 31,000 25,000 125,000 12,900
306 D 60 51 60 150 280 60 43,000 35,000 175,000 20,600
306 D 75 65 75 180 340 70 62,000 50,000 250,000 35,900
306 D 87 76 87 210 400 85 93,000 75,000 375,000 59,500
306 D 100 89 100 240 460 100 125,000 100,000 500,000 93,000
306 D 115 102 115 260 500 120 160,000 130,000 650,000 125,000
306 D 130 110 130 290 560 130 185,000 150,000 750,000 174,000
306 D 140 120 140 320 620 150 250,000 200,000 1,000,000 248,000

Grade

Limite élastique minimum

N/mm²
(RE)

Limite à la rupture

N/mm² (RN)

Allongement % minimum

Striction % minimum

Charpy V Test de résilience

Test température C°

Valeur moyenne énergetique J. min.

3

410

690

17

50

-20

40

3S

490

770

15

50

-20

45

4

580

860

12

50

-20

50